The clamp connection test program.
METALOQ Documentation v1.0, pages 68–82. Select a page to enlarge it.
Contents 1 Background ......................................................................................................................... 3
2 Experimental Program ........................................................................................................ 3
2.1 Test Specimens ........................................................................................................... 3
2.2 Uniaxial Tension Testing .............................................................................................. 4
2.3 Instrumentation and Data Acquisition ........................................................................... 5
3 Experimental Results .......................................................................................................... 7
3.1 Specimen 1 .................................................................................................................. 8
3.2 Specimen 2 .................................................................................................................18
4 Observations ......................................................................................................................25
4.1 Observations on Component Assembly or Construction .............................................25
4.1.1 Rim-Joist ..............................................................................................................25
4.1.2 Joist .....................................................................................................................25
4.1.3 Joist to Rim-Joist connection ...............................................................................26
5 Conclusions .......................................................................................................................26
6 Next steps ..........................................................................................................................27
6.1 Modification of the Existing METALOQ System ..........................................................27
6.2 Component Behaviour Research ................................................................................27
6.3 System Behaviour Research .......................................................................................27
6.4 Project funding ............................................................................................................28
Figures Figure 2-1: Joist section cut to length prior to testing ...................................................... 3 Figure 2-2: Rim-joist prepared for testing ........................................................................ 4 Figure 2-3: Specimen testing frame ................................................................................ 5 Figure 2-4: Digital Image Correlation system .................................................................. 6 Figure 3-1: Digital extensometers measuring slip in connections using digital image correlation techniques ..................................................................................................... 7 Figure 3-2: Tension force vs. connection slip for two tension members .......................... 8 Figure 3-3: Tension force vs. connection slip focused on elastic region ......................... 8 Figure 3-4: Specimen 1 orientation prior to testing .......................................................... 9 Figure 3-5: Specimen 1 force-displacement response .................................................. 10 Figure 3-6: Image pairs of Specimen 1 at identified points............................................ 11 Figure 3-7: Longitudinal strain fields on Specimen 1 at various points of response. ..... 13 Figure 3-8: Specimen 1 at failure state with connection hardware still installed ............ 13 Figure 3-9: Specimen 1 connection location showing connection slip and block shear failure of joist ................................................................................................................. 14 Figure 3-10: Backer plate of Specimen 1 connection after test ..................................... 15 Figure 3-11: Specimen 1 connection bolts after test ..................................................... 15 Figure 3-12: Specimen 1 shear tab to rim-joist connection ........................................... 16 Figure 3-13: Specimen 1 joist following test .................................................................. 16 Figure 3-14: Rim-joist of specimen 1 after test .............................................................. 17 Figure 3-15: Specimen 2 orientation prior to testing ...................................................... 18 Figure 3-16: Specimen 2 force-displacement response ................................................ 19 Figure 3-17: Image pairs of Specimen 2 at identified points .......................................... 20 Figure 3-18: Longitudinal strain fields on Specimen 2 at various points of response. ... 21 Figure 3-19: Specimen 2 at failure state with connection hardware still installed .......... 22 Figure 3-20: Specimen 2 connection location showing connection slip and block shear failure of joist ................................................................................................................. 23 Figure 3-21: Backer plate of Specimen 2 connection after test ..................................... 23 Figure 3-22: Specimen 2 connection bolts after test ..................................................... 24 Figure 3-23: Specimen 2 shear tab to rim-joist connection ........................................... 25 Tables Table 3-1: Connection slip and tension force for Specimen 1 ......................................... 9 Table 3-2: Connection slip and tension force for Specimen 2 ....................................... 18 Table 6-1: Hypothetical funding projections .................................................................. 28
1 Background The Vector Meta METALOQ modular steel structure system employs a light gauge, cold formed steel joist system connected through a proprietary shear tab to a channel section rim-joist. This connection may be subjected to a variety of force demands during shipping, craning, and service live of the module. Forces on the joint could include tension or compression along the joist longitudinal axis, bending, shear, and combined loading. This program is intended to initiate a larger testing and analysis program of the METALOQ system by testing the joist to rim-joist connection under tension loads to failure. In doing so, these tests will identify failure modes and identify any potential improvements that may be incorporated in the design.
2 Experimental Program Testing of the joist to rim-joist connections was conducted in the University of New Brunswick Civil Engineering labs. The test setup is described below. 2.1 Test Specimens Two sections of joist were cut at 50” (1270mm) in total length measured from the terminal end at the joist to rim-joist connection to the cut location (Figure 2-2). The cut location was determined based on the location of features within the joist such that there would be no interference with the mounting plate. Further consideration was made to ensure that the length was sufficiently long that shear lag effects, where the bolt forces are transferred through the section into web and flange over a length of the specimen, would not be significant at the mounting location.
Two sections of rim-joists were cut to 24” (610mm) lengths such that the shear tab was centered on the cut pieces. Four holes 1 9/16” in diameter were drilled at 18” on centre to accommodate connection of the rim-joists to the frame with threaded rods (Figure 2-2).
Test specimens were mounted to the rim-joist using the supplied connection material (backer plate and ½” fasteners) prior to testing. Tests were conducted such opposite sides of the rim-joist were visible in the optical measurements as described below. 2.2 Uniaxial Tension Testing Testing was conducted using a universal testing machine with a tension capacity of 940kN (Figure 2-3). Specimens were installed in the testing machine by clamping sections of the rim-joist to the cross-head of the testing machine with 4 high strength 1 ½” threaded rods as shown in Figure 2-2. The rim-joist sections were centered on the testing machine such that the load was concentric. Specimens were bolted into an adaptor plate using 12-½” bolts as shown in Figure 2-3. Specimens were tested using a displacement rate of 2mm/minute and tests continued until resistance of the specimens
dropped to 10% of the ultimate capacity, approximately 20 minutes after the start of the test.
2.3 Instrumentation and Data Acquisition Prior to testing, a speckle pattern of contrasting white background and black speckled paint was applied to the surface (Figure 2-4.). The speckle pattern allows for the use of digital image correlation (DIC) techniques to monitor the response of the specimen as it is loaded. DIC is an optical tracking technique that uses pattern recognition to track the
strain and displacement fields of an object. In this case, this was done using a 3D DIC system that employed two 5MP cameras mounted to a rigid rack at a fixed angle (Figure 2-4). These cameras were focused on the specimen and then the aperture was adjusted to provide a large depth of field of in-focus objects that encompass the visible region of the specimens. The camera system was then calibrated using a calibration plate that was imaged at approximately 60 different orientations within the shared field of view of the cameras (Figure 2-4). The known dimensions of patterns on the calibration plate are then used to calibrate dimensions of the visible field of view of the cameras. Once testing is complete, analysis of the images allows the computation of displacements and strain fields at all times during response. In this testing program, image pairs (one from each camera) were recorded every 1 second over the duration of the test (approximately 1200 seconds). Results of the DIC monitoring are presented later in terms of connection slip and strain fields.
3 Experimental Results A set of virtual extensometers were added to the image correlation analysis results to monitor the connection slip in the tension members during testing. The placement of these gauges is shown in Figure 3-2.
Figure 3-3 shows the tension force-connection slip behaviour for both specimens over the whole range of response. Individual specimen behaviours are discussed below, however the following generally applies:
• Specimens responded elastically up to approximately 12kN tension force
• Following the elastic limit, the response softened with a nonlinear force- displacement relationship up to a maximum between 50 and 55kN
• Following maximum force, the capacity dropped linearly as the connection failed
The elastic response of both specimens is shown in Figure 3-3. In this figure, it is evident that the elastic capacity of the connection was overwhelmed at approximately 12kN tension force. Further discussion on this is presented below.
3.1 Specimen 1 Specimen 1 was tested in an orientation such that the shear tab welded to the rim-joist was visible to the digital image correlation camera system as shown in Figure 3-4.
The tension force – connection slip relationship for specimen 1 is shown in Figure 3-5. In this figure, several points of interest have been identified and named. These points are as follows with force and displacement data listed in Table 3-1:
1A – Limit of elastic response in connections 1B – Point of significant softening in response 1C – Point of maximum tension force 1D – Point on resistance decay curve 1E – Point at end state of test with near complete fracture
Specimen 1 1A 1B 1C 1D 1E Slip (mm) 0.23 4.4 14.1 25.7 32.8 Force (kN) 14.4 45.1 54.9 23.0 7.5
The image pairs of Specimen 1 from both cameras used in the DIC analysis for the points identified in Figure 3-5 are shown in Figure 3-6. Careful examination of these images will show the connection slip becoming visually evident at around Point 1C with the detent on the joist becoming visible having slipped from the connection in Points 1D and 1E.
The longitudinal strains, those in the direction coincident with the tension force, are shown as strain field contours mapped on the deformed specimen at various points in Figure 3-7. The limits of the contour scale were set to the approximate yield strain of the steel material used in these components (2000 micro strain) with red being the tension limit and purple the compression limit. As can be seen, the tension limit is approached quickly in the shear tab connection at the elastic limit shown in b) and the high strain in the connection continues as the specimen continues to see increased load in c) and d). As the specimen is unloaded in e) and f), there remains residual strain in the shear tab indicating some permanent damage to the angle. However, this permanent damage was not evident in visual inspection.
The longitudinal strain in the joist is observed to exceed the tension limit in several points, however most of the joist damage was concentrated to the connection location that was hidden from view by the shear tab. It is evident that the strain distribution in the joist is fairly uniform at all times, with only minor stress concentrations. This indicates that the detent connection system effectively transfers connection force into the joist in an efficient manner.
d) Point 1D e) Point 1E Figure 3-7: Longitudinal strain fields on Specimen 1 at various points of response.
As the connection progressed to failure, the joist detent slipped out of the shear tab detent. This was facilitated by the bending of the backing plate as shown in Figure 3-8. In this figure, the paint line is visible on the joist showing the magnitude of slip at the failure stated. Note that the shear tab remained visually intact and did not appear to deform significantly during the test.
a) showing shear tab b) showing backing plate Figure 3-8: Specimen 1 at failure state with connection hardware still installed
Figure 3-9 shows the slip of the joist against the backer plate along with the shear block failure mode that ultimately lead to failure of the joist. In this shear block mode, b, the four shear planes that the bolt induced on the joist are shown and shear plugs are shown either detached or loosely attached to the joist. This mode is expected for tension members with widely spaced bolt lines. Close examination of Figure 3-9b also shows that the detent was flattened by action of the shear tab and the backing plate on the joist during the test. This flattening of the detent along with the bending of the backing plate facilitated the slip and the block shear of the joist. The coincident combination of these three actions resulted in the non-linear response of the connection up to the maximum resistance.
a) with backer plate in place b) backer plate removed Figure 3-9: Specimen 1 connection location showing connection slip and block shear
Figure 3-10 shows the backer plate of the connection after the test. A significant bend about the axis formed between the fastener holes is present. This bend facilitated the connection slip between the joist and the shear tab of the rim-joist.
The two ½” bolts used in the connection of Specimen 1 are shown in Figure 3-11. The bolts were largely undamaged with no signs of bolt shear. The bolts were subjected to bearing forced on the threads where the joist, shear tab, and backer plate were in contact with the bolt. The threads in the bearing area were damaged to the point that the nut would not freely spin on the bolt without the use of tools. The bolts appear to have sufficient capacity for this application.
The shear tab and rim-joist are shown in Figure 3-12 during (a) and after (b) testing. During testing there is a visible gap between the shear tab and the rim-joist in the locations between the welds when the tab is under load. This gap closed after load was removed. There was no visual damage to the shear tab nor the tab to rim-joist connection after testing.
a) Front view during test under load b) back view after test Figure 3-12: Specimen 1 shear tab to rim-joist connection
The tested Specimen 1 is shown as removed from the testing frame in Figure 3-13. In this figure, the undamaged joist outside the connection location is evident. In the connection location, the detent was largely flattened, and the double shear plane block shear failure is evident.
The rim-joist of Specimen 1 after testing is shown in Figure 3-14. There was no apparent damage to the rim-joist after testing including no visible permanent deformations and no damage to the shear tab welds on the underside of the rim-joist.
a) underside showing shear tab welds b) side view Figure 3-14: Rim-joist of specimen 1 after test
3.2 Specimen 2 Specimen 2 was tested in an orientation such that the shear tab welded to the rim-joist was not visible to the digital image correlation camera system as shown in Figure 3-15.
The tension force – connection slip relationship for Specimen 2 is shown in Figure 3-16. In this figure, several points of interest have been identified and named. These points are as follows with force and displacement data listed in Table 3-2:
2A – Limit of elastic response in connections 2B – Point of significant softening in response 2C – Point of maximum tension force 2D – Point on resistance decay curve 2E – Point at end state of test with near complete fracture
Specimen 1 2A 2B 2C 2D 2E Slip (mm) 0.22 5.0 16.4 30.0 36.4 Force (kN) 12.3 41.3 51.6 10.4 4.7
The image pairs of Specimen 2 from both cameras used in the DIC analysis for the points identified in Figure 3-16 are shown in Figure 3-17. Careful examination of these images will show the rotation of the backing plate becoming visually evident at around Point 2C with a significant opening at the top of the backing plate visible by Point 2E. The joist to rim-joist slip becomes visually observable at Point 2D with significant slip evident by Point 2E.
The longitudinal strains, those in the direction coincident with the tension force, are shown as strain field contours mapped on the deformed specimen at various points in Figure 3-18. The limits of the contour scale were set to the approximate yield strain of the steel material used in these components (2000 micro strain) with red being the tension limit and purple the compression limit. As can be seen, unlike the view of the shear tab in Specimen 1, the view of the backer plate does not demonstrate as significantly variable strains over the width. The backer plate shows a fairly uniform strain distribution that is indicative of bending stresses across the width of the plate. The longitudinal strain in the joist is observed to exceed the tension limit in several points, however most of the joist damage was concentrated to the connection location that was hidden from view by the backer plate. It is evident that the strain distribution in the joist is fairly uniform at all times, with only minor stress concentrations. This indicates that the detent connection system effectively transfers connection force into the joist in an efficient manner.
d) Point 2D e) Point 2E Figure 3-18: Longitudinal strain fields on Specimen 2 at various points of response.
As the connection progressed to failure, the joist detent slipped out of the shear tab detent. This was facilitated by the bending of the backing plate as shown in Figure 3-19. In this figure, the bolt holes and failure planes are visible on the joist showing the magnitude of slip at the failure stated. Note that the shear tab remained visually intact and did not appear to deform significantly during the test.
a) showing shear tab b) showing backing plate Figure 3-19: Specimen 2 at failure state with connection hardware still installed
Figure 3-20 shows the slip of the joist against the backer plate along with the shear block failure mode that ultimately lead to failure of the joist. In this shear block mode, b, the four shear planes that the bolt induced on the joist are shown and shear plugs are shown either detached are loosely attached to the joist. This mode is expected for tension members with widely spaced bolt lines. Close examination of Figure 3-20b also shows that the detent was flattened by action of the shear tab and the backing plate on the joist during the test. This flattening of the detent along with the bending of the backing plate facilitated the slip and the block shear of the joist. The coincident combination of these three actions resulted in the non-linear response of the connection up to the maximum resistance.
a) with backer plate in place b) backer plate removed Figure 3-20: Specimen 2 connection location showing connection slip and block shear
Figure 3-21 shows the backer plate of the connection after the test. A significant bend about the axis formed between the fastener holes is present. This bend facilitated the connection slip between the joist and the shear tab of the rim-joist.
The two ½” bolts used in the connection of Specimen 2 are shown in Figure 3-22. The bolts were largely undamaged with no signs of bolt shear. The bolts were subjected to bearing forced on the threads where the joist, shear tab, and backer plate were in contact with the bolt. The threads in the bearing area were damaged to the point that the nut
would not freely spin on the bolt without the use of tools. The bolts appear to have sufficient capacity for this application.
The shear tab and rim-joist is shown in Figure 3-23 during (a) and after (b) testing. During testing there is a visible gap between the shear tab and the rim-joist in the locations between the welds when the tab is under load. This gap closed after load was removed. There was no visual damage to the shear tab nor the tab to rim-joist connection after testing.
4 Observations In addition to the information provided above, the following observations were made: 4.1 Observations on Component Assembly or Construction 4.1.1 Rim-Joist • The joist to rim-joist connection employed a shear tab that was welded to the rim- joist with a non-continuous fillet weld on the back side of the rim-joist.
signs of failure. • The shear tab was bent approximately 90º at the edge of the tab presumably to add rigidity and reduce potential tab rotation under load. This is likely more significant for shear or flexure loads than for tension loads.
o The shear tabs appeared undamaged from the testing. • The detent on the rim-joist was formed to mate with the detent on the joist and the backing component of the rim-joist to joist connection. This detent served an apparent function to transfer force from the joist to the tab through a large bearing area. The performance of this component is discussed further in following sections.
o The detent on the shear tab was apparently undamaged during testing. • The rim-joist was constructed of a channel section bent from steel plate. o There was deformation of the wall of the web of the channel at the location
of the tab during testing, but full recovery of deformation was observed with no apparent damage to the channel.
4.1.2 Joist • The joist was a commercially available, cold formed, galvanized steel joist bent to a wide flange “I”.
o Outside of the connection location the joist was undamaged during testing. • The joist was connected to the shear tab with two ½”-13 bolts and a detent system for bearing
failure occurred that included both the slipping and flattening of the joist detent and the bolted connection failure in a shear block mode with four shear planes. The shear block failure mode, where the bolts pull through the steel material, is expected in a tension connection of this configuration (neglecting the detents). • The detent system appeared to be designed to increase bearing area on the joist o The digital image correlation analysis showed a very uniform distribution of
longitudinal strain over the width of the joist. There was very little apparent shear lag, where concentrated forces are slowly distributed over the member. The detent system appeared to function well to transfer bearing forces to the joist up to the elastic limit and through the progression of failure.
4.1.3 Joist to Rim-Joist connection • A series of mated parts connected together with two ½”-13 bolts o The bolts were largely undamaged during testing, however the threads at
the bearing locations were damaged to the point where the nut would no longer spin on the bolt. Structurally, the bolts appeared sufficient for this application. • The mated detent system appeared designed to transfer bearing forces from the joist to the shear tab over a wide area of the joist web.
o This system appeared to fail progressively during testing. o The initial response was stiff as the full bearing of the detent on the joist and
the bolts was present. o At a relatively small slip between the joist and the shear tab of approximately
0.2mm at 12kN in tension, the system began to soften. o This softening continued to approximately 15mm slip where maximum
resistance was achieved of approximately 51kN in tension. o As the system moved up to maximum load, a combination of flattening of
the joist detent system, bending of the thick-walled backing detent system, and block shear of the bolts through the joist occurred. • The thick-walled backing plate that mates into the detent system was apparently intended to act as a washer and to clamp the joist detent into the shear tab detent.
component occurred. The backer piece bent about an axis that is formed between the two bolts in the system. This bending allowed the joist detent to deform and to slip out of the shear tab detent in the progression of failure.
• The system is stiff and elastic up to approximately 12kN at approximately 0.2mm slip between joist and shear tab.
• The system responded inelastically for the majority of the response with increasing resistance and decreasing stiffness up to approximately 52kN at approximately 15mm slip.
• The bending of the thick-walled backer plate allowed slip between the detents resulting in a loss of bearing.
• The detent system transferred stress (through strain measurements) with fairly uniform distribution over the joist width.
• The bolts are sufficient for this application.
• The tension member ultimately failed in a block shear mode with four shear planes as expected. This mode is likely for a two bolt-line connection into the web of a flanged tension member and is neither good nor bad.
• The rim-joist was undamaged.
• The shear tab was undamaged.
6 Next steps Future work of the following nature is proposed for the METALOQ system: 6.1 Modification of the Existing METALOQ System From this preliminary testing, it is apparent that there was a significant difference between the elastic limit of the system (approximately 12kN tension) and the ultimate limit (approximately 52kN tension). This significant difference appeared to be the result of the progressive failure mechanism of the slipping of the joist detent from the shear tab detent and the accompanying shear block failure of the bolts on the joist material. Based on the digital image correlation strain observations, the detent system functioned exceptionally well in distributing load over the joist, indicating that the shear block failure was not the driving mode of failure. Instead, based on these two tests alone, it appears that the thick- walled backer plate on the connection contributed to early damage in the connection. The bending of the plate allowed the joist to slip from the detent and the progression of failure. It is possible that stiffening this plate against this mode will increase the elastic capacity of the system and potentially increase the ultimate capacity as well. Although this conclusion is only based on tension testing, it is likely to be similar for compression and flexure as well. This stiffening may not be a benefit to shear performance. It should be noted that the image correlation did show significant strains in the shear tab that approached (and potentially exceeded in local areas) the material yield strain. Stiffening and strengthening the bent plate backing washer to increase capacity may expose a new failure mode in the shear tab system. However, if this were the case, this mode would have inherently higher strength than the existing system. 6.2 Component Behaviour Research A series of experimental tests should be conducted on individual components or component sub-systems including in part:
• Joist to rim-joist connection under o shear o bending o combined loading o compression o tension (continuation of this work)
• Column to beam connection
• Columns under compression
• Columns under combined loads
6.3 System Behaviour Research Following, or in parallel with the component testing, system limit states testing should be conducted on:
• Floor system behaviour under different gravity loading configurations • Wall racking under lateral loads
• Module torsion
• Module racking
• Multi-module lateral load, gravity load, and torsional load testing
• Testing of critical devastations from typical modular system such as those around elevator shafts and stair wells.
• Testing of system response to progressive collapse
In addition to the ultimate capacity testing of components and systems, testing that focuses on the following items should be considered:
• Service vibrations for occupancy
• Vertical and lateral deflection limits for occupancy
• Building envelope testing against water and air ingress, cyclic pressures, thermal cycles, and windborne debris impacts.
In addition to experimental testing, finite element modeling of the structure or components is recommended.
METALOQ Conclusion: Based on the test results and failure analysis, the standard clamp plate has been thickened to further increase connection capacity.
This section is an orientation to the METALOQ system. It does not replace project-specific architecture or engineering, and nothing here should be relied on to design a building. Every project needs licensed professionals and the approval of the authorities having jurisdiction. Illustrations are not to scale.